Thaum tshav kub kub-resistant phlogolite mica phaj muaj cov tuab tuab, cov khoom siv hluav taws xob zoo thiab lub zog txhua yam;nws yog ib yam tshiab ntawm hluav taws xob thiab thermal insulating khoom board.Lub sij hawm ntev ua hauj lwm kub ntawm phlogopite board yog 800 ℃, thiab lub thickness ntawm feem ntau siv mica board yog nruab nrab ntawm 0.1-1.0mm
Cov khoom siv hluav taws xob kub zoo heev, qhov kub siab tshaj plaws tiv thaiv mus txog 1000 ℃.
Kev ua tau zoo ntawm hluav taws xob rwb thaiv tsev, kev tiv thaiv hluav taws xob tawg qhov ntsuas ntawm cov khoom zoo tib yam yog siab li 20KV / mm.
Zoo heev flexural zog thiab kev ua tau zoo, cov khoom muaj siab flexural zog thiab zoo heev toughness, thiab tuaj yeem ua tiav rau hauv ntau yam tshwj xeeb-puab qhov chaw los ntawm lathes, milling machines thiab drilling tshuab yam tsis muaj delamination.
Tsawg thermal conductivity, zoo heev hluav taws xob rwb thaiv tsev zog, roj thiab corrosion kuj, asbestos hloov.
Phlogolite mica phaj dav siv hauv cov tshuab plaub hau, toasters, irons, heaters, rice cookers, ncu, rice cookers, heaters, microwave ncu, heating and heat insulation and other electronic products.
Khoom Lub Npe | Mica nrog Fiber iav Cloth ntawm ob sab |
MICA | Phlogopite |
Ntev (m) | 20-100 |
Dav (m) | 1 |
Thickness (hli) | 0.2-0.8 hli |
Mica Cov ntsiab lus (%) | 83 ib |
Cov ntsiab lus iav (%) | 8 ~ 10 |
Cov ntsiab lus Binder (%) | 8 ~ 10 |
Tensile zog (N / 15mm) | 400 |
Dielectric zog (KV) | > 4.0 |
Thermal conductivity (W / mK) | 0.3 |
Thermal Expansion (10-6 / K) | 100 |
Thaum tshav kub kub conductivity (W / mK) | 3 |
Tracking Index(v) | 525 |
Qib hluav taws kub (℃) | 750-800 Nws |
Oxygen Index | 90 |
Tsom ntsoov rau kev muab cov kev daws teeb meem mong pu rau 5 xyoos.